Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 0850-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable E1330I Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JD455CJ Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable Y283 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R7831A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WJAF111L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 1490 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1490 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Chevron Phillips HiD® 9352 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: corrugated pipe applicationsInformation provided by Chevron .. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Chevron Phillips HiD® 9354 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymerApplications: corrugated pipe applicationsInformation provided by Chevron Phillips Chemical Company. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman M3006-P Polyethylene
(discontinued **) Medium density polyethylene M3006-P is a specialty formulation suggested for high speed extrusion coating applications. M3006-P offers improvements over low density polyethylene in barrier properti.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R3790B Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa @Temperature 23.0 °C |
2390 psi @Temperature 73.4 °F |
ISO 527-2/50 |
MBA Polymers PP 2182 Post-consumer recycled polypropylene copolymer Very high melt flow rate for injection molding application. Available in standard black.Information provided by MBA Polymers. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | 100% elongation |
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Chevron Phillips Marlex® 5104 LDPE Blow Molding Resin Resin Type: HomopolymerCharacteristics: High Melt Strength, Good Parison Control, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on Gloss, Long Standing .. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMU130P Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci.. |
|||
Tensile Strength, Yield | 16.5 MPa @Strain 300 % |
2390 psi @Strain 300 % |
ASTM D412 |
Dow Buna® SB 1500 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1500 - Schkopau is manufactured by cold polymerization using a rosin acid soap. A discoloring stabilizer is added during the production process. Buna® SB 1500 - Schkopau is a general pu.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Molded property |
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ISO 527-1/-2 |
DSM Arnitel® UM551-V Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 16.5 - 31.0 MPa | 2390 - 4500 psi | Average value: 23.3 MPa Grade Count:116 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ISO 527-1/-2 |
DSM Arnitel® UM551-V 55 Shore D, Flame Retardant (halogen-, phosphorous-free) Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Syncure™ System S117FH Polyethylene, Crosslinked (XLPE) NOTE: The above represents Typical Properties measured on 20 AWG with 16 mil wall. STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap.Information provided .. |