Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 13.1 MPa | 1900 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JC404HX Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WJKC505L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | |
Resinlab® CYNERGY CA6601 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | |
Resinlab® CYNERGY CA6602 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | |
Resinlab® CYNERGY CA6702 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D638 |
M. Holland Company LL700 LLDPE
(discontinued **) Features: High ESCR (Stress Crack Resist.), Good Flexibility, High FlowUses: Closures, Household GoodsProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer Chemraz® SD625, a black-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resistance a.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® D 4107 C Black TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good I.. |
|||
Tensile Strength, Yield | >= 13.1 MPa | >= 1900 psi | ASTM D-882 |
Saint-Gobain Norton® T-200 Mechanical Grade PTFE Sheet (0.031" thick) Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate release sheets, .. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3201-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D412 |
Teknor Apex APEX® 3210-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D412 |
Teknor Apex APEX® 3301-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3310-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D412 |
Teknor Apex APEX® 90-A41R-70-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | Longitudinal |
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.005" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | transverse direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | 100% Retention, Hot Air Aging, 22 hrs at 70°C |
Teknor Apex UNIPRENE® 7400-40D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | 2"/min; ASTM D638 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | transverse direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | transverse direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D-638 |
Axiall 50897 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D-638 |
Axiall 6730 Moldings & Extrusions Flexible PVC Injection molding compound with good processing characteristics that allow fast cycles and smooth unblemished surfaces on the finished product. Exhibits good weathering and low temperature properti.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D-638 |
Axiall 10641 Wire & Cable Flexible PVC Non-lead stabilized general purpose jacket compound designed for good flexibility and good low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D-638 |
Axiall 19840 Wire & Cable Flexible PVC 105°C rated insulation suitable for 1/64 wall. Recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | ASTM D-638 |
Axiall 18752 Wire & Cable Flexible PVC Electrical grade extrusion compound with excellent low temperature performance. Maximum service temperature of 105°CInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
Tensile Strength, Yield | 13.1 MPa | 1900 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman D4041-P Polyethylene
(discontinued **) Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in an.. |