Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.31 MPa
190 psi
at 200%, as molded
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.31 MPa
190 psi
ASTM D412
Polymax® Maxelast® P3965H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 1.31 MPa
190 psi
@50% Elongation; ASTM D1414
Greene Tweed FLUORAZ® 888 Fluoroelastomer, FEPM
Fluoraz® 888 polytetrafluoroethylene/propylene (FEPM) performs well in aggressive chemicals where ultra pure materials are not required. Recommended for conventional wet and dry system applicatio..
Tensile Strength, Yield 1.31 MPa
190 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.31 MPa
190 psi
200%, post cured- 8 hours at 177°C; ASTM D412
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.31 MPa
190 psi
at 100%; ASTM D638
Multibase Multi-Flex® A 6221 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Thermal Stability, GoodOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsAutomotive Under the HoodInfo..
Tensile Strength, Yield >= 1.31 MPa
>= 190 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7075 Ethylene-Propylene Rubber
General service EPDM.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield >= 1.31 MPa
>= 190 psi
Stress at Elongation M50; ASTM D412 Method A