Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 960 - 1210 MPa | 139000 - 175000 psi | |
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Tensile Strength, Yield | >= 960 MPa @Strain 0.200 % |
>= 139000 psi @Strain 0.200 % |
|
Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures Description: SUPERELSO® 960 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 960 N/mm² (140 KSI), SUPERELSO® 960 enables to make weig.. |
|||
Tensile Strength, Yield | 960 MPa @Strain 0.200 % |
139000 psi @Strain 0.200 % |
|
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 958 MPa @Strain 0.200 %, Temperature 21.1 °C |
139000 psi @Strain 0.200 %, Temperature 70.0 °F |
|
Latrobe Lescalloy® 6305 VAC-ARC ; High Strength Alloy Steel LESCALLOY 6305 VAC-ARC steel is a modified 4140 steel with higher molybdenum and a vanadium addition. The alloy steel is generally used in the 160/180,000 psi tensile strength range obtained with a.. |
|||
Tensile Strength, Yield | 958 MPa @Strain 0.200 %, Thickness 50.8 mm |
139000 psi @Strain 0.200 %, Thickness 2.00 in |
|
Latrobe Lescalloy® 6305 VAC-ARC ; High Strength Alloy Steel LESCALLOY 6305 VAC-ARC steel is a modified 4140 steel with higher molybdenum and a vanadium addition. The alloy steel is generally used in the 160/180,000 psi tensile strength range obtained with a.. |
|||
Tensile Strength, Yield | >= 960 MPa @Thickness 50.0 mm |
>= 139000 psi @Thickness 1.97 in |
|
ThyssenKrupp XABO® 960 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength, Yield | 960 MPa @Strain 0.200 % |
139000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar Low Cost, Multipurpose Alloy. Tensile property data below for Annealed Sheet/Plate & Billet/Bar.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wit.. |