Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.03 MPa | 1310 psi | ASTM D412 |
Polymax® Maxelast® A9950C TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
Precision Polymer Engineering E60D Ethylene Propylene Rubber Sulphur cured, Ethylene Propylene Terpolymer, 56-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W’. Water Research Council (WRC) teste.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ISO 527 |
Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection mo.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
Precision Polymer Engineering P90B Polyacrylate Rubber Polyacrylic or Polyacrylate Rubber, 85-95 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | -10% change after 168 hours @ 70°C; ASTM D412 |
Precision Polymer Engineering R80Z Natural Rubber Natural Rubber, 75-85 °IRHD. Formulated to meet BS1154 Grade Z80. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
Precision Polymer Engineering V75G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 70-80 °IRHD. Diesel liner ring grade. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK707, A1-10, B38, EF31, EO78, F.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
Precision Polymer Engineering E50D Ethylene Propylene Rubber Sulphur cured, Ethylene Propylene Terpolymer, 46-55 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W’. Water Research Council (WRC) teste.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE5050 Extrusion Coating Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: High draw down, low neck-in, excellent heat sealability, and excellent adhesion.Applications: Extrusion: coating grade and t.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE5080 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms to FDA regulation 21 CFR.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE 1402 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE1503 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 2012 D SW 413 LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 9.03 MPa | 1310 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 605 Perfluoroelastomer Chemraz® 605, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. A high temperature compound with superior compression set resistance, physical properties and e.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 2003 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 1804 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 1810 D LDPE Blow moldings, sheet, profile, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 1810 H LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 1840 D LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
UBE PAE1200U Nylon Elastomer Description: UBESTA Nylon 12 ElastomerInformation provided by UBE. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ISO 527-2 |
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating LDPE LA 0710 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum. High draw down, low neck in.In.. |
|||
Tensile Strength, Yield | 9.00 MPa @Strain 100 % |
1310 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
Trelleborg E550 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | 300% elongation; ASTM D412 |
Lubrizol Estane® 5712 Thermoplastic Polyurethane Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl.. |
|||
Tensile Strength, Yield | 9.00 MPa @Strain 300 % |
1310 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® 481 Polyurethane injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
Dow LDPE 4005M Low Density Polyethylene Data provided by Dow Chemical. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | 500% elongation; ASTM D412; ASTM D638 |
Lubrizol Estane® 58252 Thermoplastic Polyurethane Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE1158 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ISO R527 |
Total Lacqtene® 1025 FH 24 LDPE blown film
(discontinued **) Radical polyethylene made by high pressure tubular process. Slip and antiblock formulated grade for good transparent thin films. Advised temperature profile : 150 to 190°C.Information provided prov.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE1353 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |