Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 873 MPa | 127000 psi | at Surface, Transverse |
International Mold Steel P20 Plastic Mold Steel P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel.
Information provided by International Mold Steel. |
|||
Tensile Strength, Yield | 873 MPa | 127000 psi | at Surface, Longitudinal |
International Mold Steel P20 Plastic Mold Steel P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel.
Information provided by International Mold Steel. |
|||
Tensile Strength, Yield | 873 MPa | 127000 psi | at Center, Longitudinal |
International Mold Steel P20 Plastic Mold Steel P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel.
Information provided by International Mold Steel. |
|||
Tensile Strength, Yield | 876 MPa @Strain 0.200 % |
127000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 875 MPa @Strain 0.200 % |
127000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals INCONEL® Alloy 751 A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-.. |
|||
Tensile Strength, Yield | 875 MPa @Strain 0.200 % |
127000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals NIMONIC® Alloy 901 A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at .. |
|||
Tensile Strength, Yield | 876 MPa @Strain 0.200 % |
127000 psi @Strain 0.200 % |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
Tensile Strength, Yield | 876 MPa | 127000 psi | Long. |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |