Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 51.7 - 88.3 MPa | 7500 - 12800 psi | Average value: 65.7 MPa Grade Count:3 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Yield | 28.0 - 88.3 MPa | 4060 - 12800 psi | Average value: 59.4 MPa Grade Count:38 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |