Mechanical Properties Metric English Comments
Tensile Strength, Yield 370 - 560 MPa
53700 - 81200 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Yield 480 - 560 MPa
69600 - 81200 psi
Solution Annealed and Aged
Materion Beryllium Copper Alloy 10C Castings (UNS C82000)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchTabul..
Tensile Strength, Yield 410 - 560 MPa
59500 - 81200 psi
Materion Beryllium Copper Alloy 25 Strip; 1/4 H (TD01) Temper (UNS C17200)
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 62-75Tabulated properties apply ..
Tensile Strength, Yield 510 - 560 MPa
74000 - 81200 psi
L direction
ArcelorMittal Speed 35-510 Electrical Steel
Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 370 - 560 MPa
53700 - 81200 psi
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..