Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 380 - 550 MPa @Strain 0.200 % |
55100 - 79800 psi @Strain 0.200 % |
|
Kobe Steel KS70 Commercially Pure Titanium, ASTM Gr. 3, Annealed Nominal Composition: Ti-Fe-OApplications: Tube sheets.Features: Relatively high strength, excellent corrosion resistance.Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 450 - 550 MPa @Strain 0.200 % |
65300 - 79800 psi @Strain 0.200 % |
|
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Yield | 450 - 550 MPa | 65300 - 79800 psi | |
ArcelorMittal Dual Phase 780 LCE Y450 Very high strength steel, Cold Rolled Steel Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft .. |
|||
Tensile Strength, Yield | 460 - 550 MPa | 66700 - 79800 psi | |
ArcelorMittal HSLA 460 High strength low alloy steel for cold forming, Hot Rolled Available in the following: S460MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w.. |
|||
Tensile Strength, Yield | 460 - 550 MPa | 66700 - 79800 psi | |
ArcelorMittal TRIP 780 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT780T), electrogalvanized (HCT780T+ZE) and Extragal®/Galvannealed (HCT780T+Z/+ZZF)Description: TRIP steels offer an outstanding combination of strength and d.. |
|||
Tensile Strength, Yield | 350 - 550 MPa | 50800 - 79800 psi | before hot stamping |
ArcelorMittal Usibor® 1500 Ultra high strength steel, Cold Rolled Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to .. |
|||
Tensile Strength, Yield | 350 - 550 MPa | 50800 - 79800 psi | before hot stamping |
ArcelorMittal Usibor® 1500 Ultra high strength steel, Hot Rolled Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to .. |
|||
Tensile Strength, Yield | 450 - 550 MPa | 65300 - 79800 psi | |
ArcelorMittal Dual Phase 780 Y450 Very high strength steel, Cold Rolled Steel Available in the following: HCT780X (uncoated), HCT780X+ZE (electrogalvanized) and HCT780X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |
|||
Tensile Strength, Yield | 320 - 550 MPa | 46400 - 79800 psi | before hot stamping |
ArcelorMittal Usibor® 22MnB5 Ultra high strength steel, Cold Rolled Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to .. |
|||
Tensile Strength, Yield | 320 - 550 MPa | 46400 - 79800 psi | before hot stamping |
ArcelorMittal Usibor® 22MnB5 Ultra high strength steel, Hot Rolled Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to .. |