Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.3 - 22.5 MPa | 1490 - 3260 psi | ISO/R 527E |
Mikro-Technik Reproflon PTFE Reproflon is reclaimed PTFE scraps. The powder can be reused for the usual manufacturing procedures.Information provided by Mikro-Technik GmbH |