Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ISO 527 |
Polimeri Europa Flexirene® MS 20 A Linear Low Density Polyethylene Flexirene MS 20 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 A are characterized by optimum low tempe.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ISO 527 |
Polimeri Europa Flexirene® MS 20 U Linear Low Density Polyethylene Flexirene MS 20 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 U are characterized by optimum low tempe.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ISO 527 |
Polimeri Europa Flexirene® MS 26 A Linear Low Density Polyethylene Flexirene MS 26 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 26 A are characterized by optimum low tempe.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ISO 527 |
Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection mo.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
Precision Polymer Engineering N60C Nitrile Rubber Nitrile Butadiene Rubber (NBR). High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class "C", 55-65 IRHD. Approval ref.: 31/6.1... |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
Precision Polymer Engineering N70C Nitrile Rubber Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class D, approval ref.: 31/6.1... |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
Precision Polymer Engineering S50H Silicone Rubber White Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States F.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
Precision Polymer Engineering E50D Ethylene Propylene Rubber Sulphur cured, Ethylene Propylene Terpolymer, 46-55 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W’. Water Research Council (WRC) teste.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ISO 527 |
Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for inject.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman 811E Polyethylene
(discontinued **) Extrusion grade; no additives. 811E as supplied by Eastman Chemical may lawfully be used in food contact (noncooking) subject to FDA 21 CFR 177.1520(c)(2.1).Information from manufacturer data sheet.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE5050 Extrusion Coating Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: High draw down, low neck-in, excellent heat sealability, and excellent adhesion.Applications: Extrusion: coating grade and t.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE5080 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms to FDA regulation 21 CFR.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE1155 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA Copolymer and FDA compliant.Features: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications:.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE1503 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Tensile Strength, Yield | 9.00 - 33.0 MPa | 1310 - 4790 psi | Average value: 26.5 MPa Grade Count:6 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 2012 D SW 413 LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 2003 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | >= 9.00 MPa | >= 1310 psi | |
Kazanorgsintez PE2NT 15-10 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Tensile Strength, Yield | >= 9.00 MPa | >= 1310 psi | |
Kazanorgsintez PE2NT 16-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
LyondellBasell Lupolen® 1840 D LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
UBE 7128B Nylon 6/12 Copolymer Description: UBESTA Nylon 12 CopolymerInformation provided by UBE. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
UBE PAE1200U Nylon Elastomer Description: UBESTA Nylon 12 ElastomerInformation provided by UBE. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
Trelleborg E669 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | |
Trelleborg E666 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | 2 in/min, Type IV bar; ASTM D638 |
Chevron Phillips Marlex® 1003 LDPE Injection Molding Resin Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: HousewaresTamper evident, snap-on capsWine bottle sleeve capsInfo.. |
|||
Tensile Strength, Yield | 9.00 MPa @Strain 300 % |
1310 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1485A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldingvery large processing windowhigh melt stabilityBeadsApplicationBellowsHosesnon-reinforcedProfilesInjection molded engineering.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |
|||
Tensile Strength, Yield | 9.00 MPa @Strain 100 % |
1310 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE1451 EVA Film Extrusion
(discontinued **) 4.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D638 |
Huntsman PE2049 Injection Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good molding processability, produces parts that are flexible, and show excellent flatness in large projected areas.Applicat.. |