Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 483 MPa @Temperature 23.9 °C |
70000 psi @Temperature 75.0 °F |
ASTM D3039 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Tensile Strength, Yield | 483 MPa @Temperature 23.9 °C |
70000 psi @Temperature 75.0 °F |
ASTM D638 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Tensile Strength, Yield | >= 483 MPa | >= 70100 psi | 0.2% proof |
Kobe Steel KS3-2.5 Alpha-Beta Titanium Alloy, ASTM Gr. 9, Annealed Nominal Composition: Ti-3 Al-2.5 V Applications: Exhaust systems, bicycle frames, eye glass frames.Features:High strength, excellent balance between strength and toughness.Information provided by K.. |
|||
Tensile Strength, Yield | 483 - 655 MPa | 70100 - 95000 psi | 0.2% proof |
Kobe Steel KS85 Commercially Pure Titanium, ASTM Gr. 4, Annealed Nominal Composition: Ti-Fe-OApplications: Airplane Parts.Features: Relatively high strength, excellent corrosion resistance.Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 483 - 517 MPa @Strain 0.200 % |
70000 - 75000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 483 - 517 MPa @Strain 0.200 % |
70000 - 75000 psi @Strain 0.200 % |
|
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 483 - 552 MPa @Strain 0.200 % |
70000 - 80000 psi @Strain 0.200 % |
|
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 483 MPa @Strain 0.200 %, Temperature 93.0 °C |
70100 psi @Strain 0.200 %, Temperature 199 °F |
|
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 483 MPa | 70000 psi | ASTM D-638 |
Glastic SG-200 Corner Angles Corner angles used for coil winding.Information provided by Glastic Corporation |
|||
Tensile Strength, Yield | 483 - 517 MPa @Strain 0.200 % |
70000 - 75000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 483 - 896 MPa | 70000 - 130000 psi | |
Meehanite Ductliron® SH-100 Nodular Graphite Ductile Iron Type SP-100 is characterized by its exceptional hardenability. It is particularly suited where high strengths are desired in relatively heavy casting sections. In the as-cast condition it has a pe.. |
|||
Tensile Strength, Yield | 483 - 689 MPa @Strain 0.200 %, Thickness <=25.4 mm |
70000 - 100000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Tensile Strength, Yield | 483 - 689 MPa @Strain 0.200 % |
70000 - 100000 psi @Strain 0.200 % |
Escomatic Coils |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Tensile Strength, Yield | 483 - 689 MPa @Strain 0.200 %, Thickness <=25.4 mm |
70000 - 100000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Tensile Strength, Yield | >= 483 MPa | >= 70100 psi | |
ThyssenKrupp X8Ni9 Structural Steel Data applies to plate thicknesses from 13/64 to 1 15/64 in.9% nickel steel for low temperature service down to -320°FApplication for pressure vessels and tanks for the transportation and storage of.. |
|||
Tensile Strength, Yield | 483 MPa | 70000 psi | Annealed and Aged |
Universal Wire Works Inconel 92 (AMS 5675) Nickel Alloy Filler Metal Inconel Filler Metal 92 is a nickel base alloy designed especially for gas tungsten arc and gas metal arc welding of dissimilar combinations of high nickel alloys and austenitic and ferritic steels... |
|||
Tensile Strength, Yield | >= 483 MPa | >= 70100 psi | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.Features.. |
|||
Tensile Strength, Yield | 483 MPa | 70000 psi | |
Universal Wire Works 70S-2 Steel Welding Wire Universal 70S-2 is designed for TIG or MIG welding of all carbon steels. The tensile strength exceeds the base metal on single pass deposits on gaged carbon steel. Alloy 70S-2 is triple deoxidized u.. |
|||
Tensile Strength, Yield | 483 - 531 MPa | 70000 - 77000 psi | 0.2% offset |
Eagle Brass 194 HSM® Copper, Extra Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Yield | 483 - 572 MPa | 70000 - 83000 psi | 0.2% offset |
Eagle Brass 511 Phosphor Bronzes 4%, Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Yield | 483 - 586 MPa | 70000 - 85000 psi | 0.2% offset |
Eagle Brass 521 Phosphor Bronzes 8% C, 3/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Yield | 483 - 517 MPa | 70000 - 75000 psi | |
Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy Finished product available as bar, wire, or rod.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Meta.. |
|||
Tensile Strength, Yield | 483 MPa | 70100 psi | Castings |
CMW® 353 Copper Alloy CMW® 353 material is an economical high strength, high conductivity copper base alloy. It is a heat treatable copper base alloy and its excellent properties are obtained largely through heat treatm.. |
|||
Tensile Strength, Yield | 483 MPa | 70100 psi | |
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Tensile Strength, Yield | 483 MPa | 70000 psi | Stress relieved |
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 483 MPa @Strain 0.200 % |
70100 psi @Strain 0.200 % |
|
Carpenter Invar 36® Alloy, Cold Drawn Bars Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Tensile Strength, Yield | >= 483 MPa | >= 70100 psi | Hardened and Tempered |
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 483 MPa @Strain 0.200 % |
70100 psi @Strain 0.200 % |
|
ATI Allvac® 70, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |
|||
Tensile Strength, Yield | 483 MPa @Strain 0.200 % |
70100 psi @Strain 0.200 % |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Tensile Strength, Yield | 483 MPa @Strain 0.200 %, Temperature 566 °C |
70100 psi @Strain 0.200 %, Temperature 1050 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |