Tensile Strength, Yield 425 MPa

@Strain 0.200 %
61600 psi

@Strain 0.200 %
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 425 MPa

@Strain 0.200 %
61600 psi

@Strain 0.200 %
Haynes 230® alloy, 0% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 425 MPa

@Strain 0.200 %
61600 psi

@Strain 0.200 %
Haynes Hastelloy® S alloy, weld metal, aged at 649°C (1200°F) for 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 425 MPa
61600 psi
Haynes Hastelloy® W alloy as a weld filler, base metal Multimet alloy 12.7 mm plate weldment
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 425 MPa

@Strain 0.200 %
61600 psi

@Strain 0.200 %
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Tensile Strength, Yield 425 MPa

@Strain 0.200 %,
Temperature 200 °C
61600 psi

@Strain 0.200 %,
Temperature 392 °F
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..
Tensile Strength, Yield 425 MPa
61600 psi
CMW® 328 Copper Alloy
CMW® 328 material is a high strength, high conductivity copper base alloy. CMW® 328 is heat treatable. Optimum mechanical and physical properties of CMW® 328 material are developed by heat treatm..
Tensile Strength, Yield 425 - 465 MPa
61600 - 67400 psi
T direction
ArcelorMittal Save 20-13 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 425 - 465 MPa
61600 - 67400 psi
T direction
ArcelorMittal Save 25-14 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 425 - 465 MPa
61600 - 67400 psi
T direction
ArcelorMittal Save 27-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 425 - 465 MPa
61600 - 67400 psi
T direction
ArcelorMittal Save 30-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 425 MPa

@Strain 0.200 %
61600 psi

@Strain 0.200 %
Haynes 625 alloy, 10% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C (1500°F), good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a var..