Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.10 MPa | 595 psi | 200%, post cured- 4 hours at 200°C; ASTM D412 |
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 4.10 MPa | 595 psi | ASTM D412 |
Polymax® Maxelast® P2950T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 4.10 MPa | 595 psi | ASTM D412 |
Polymax® Maxelast® P3740 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 4.10 MPa | 595 psi | M100 |
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good .. |
|||
Tensile Strength, Yield | 4.10 MPa | 595 psi | At 100% elongation, across flow; ASTM D412 |
Advanced Elastomer Systems VistaFlex® 715-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Tensile Strength, Yield | 4.10 MPa @Strain 100 % |
595 psi @Strain 100 % |
|
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content Features: Good mechanical characteristics.Information provided by Daikin Industries. |
|||
Tensile Strength, Yield | 4.10 MPa @Strain 100 % |
595 psi @Strain 100 % |
|
Daikin DAI-EL G-575 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 70% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low permeability to gasoline and a.. |
|||
Tensile Strength, Yield | 4.10 MPa | 595 psi | chs 20 in/min; ASTM D638 |
Diamond Polymers Softflex® 4550 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 4.10 MPa | 595 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Tensile Strength, Yield | 4.10 MPa | 595 psi | cured 72 hrs @ RT |
ACC QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material QM 245 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Tensile Strength, Yield | 4.10 MPa | 595 psi | M100 |
3M Dyneon™ Fluorel™ FC-2211 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |