Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 310 MPa | 45000 psi | |
Pacific Sintered Materials FCC-216-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
MetalTek MTEK 175-C Cast UNS C95400HT Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | |
Mueller Alloy 3530 High Leaded Brass 62% (UNS C35300) Used for screw machine products requiring some cold formability (i.e. crimping, knurling)Applications: Alloy 3530 is used for screw machine applications requiring the ability to be cold formed eithe.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 760 °C |
45000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes 242® alloy, bar and rings, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 870 °C |
45000 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 242® alloy, bar and rings, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 648 °C |
45000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 556® alloy, all-weld metal GTAW Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | Annealed |
Special Metals INCONEL® Alloy 600 A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for.. |
|||
Tensile Strength, Yield | 310 MPa @Temperature 71.0 °C |
45000 psi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Crucible Steel 410 Chromium Steel Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Cruci.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Crucible Steel 430 Chromium Steel Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | |
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536 Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
Annealed |
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
AK Steel 434 Ferritic Stainless steel AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
AK Steel 436 Ferritic Stainless steel Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 1011, Grade 45 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 607 Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel CL 1/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 045XLK SAE Specified properties not covered by ASTMInformation provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 055XLK SAE Specified properties not covered by ASTMInformation provided by AK Steel |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
Annealed |
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® HC-276 Nickel Superalloy, Heat Treatment: 1121°C (2050°F) Anneal Data provided by Allvac.Applications: High temperature applications also requiring good resistance to corrosive fluids, such as liquids and combustion products. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 1011, Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 570, Grade 45 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Yield | 310 - 379 MPa @Strain 0.200 % |
45000 - 55000 psi @Strain 0.200 % |
Annealed |
AK Steel 15 Cr-Cb® ULTRA FORM® Ferritic Stainless steel AK Steel’s 15 Cr-Cb ULTRA FORM® is a low-carbon, low-nitrogen ferritic grade of stainless steel with an intermediate, 14.5% chromium content. Alloying additions of Ti, Cb, Si and Mn provide excell.. |