Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 31.03 MPa | 4501 psi | ASTM D638 |
Lucent Polymers TPP-140 Polypropylene, Homopolymer, 40% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 31.03 MPa | 4501 psi | ASTM D638 |
Lucent Polymers PPC-0222 Polypropylene, Impact Modified Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 31.03 MPa | 4501 psi | ASTM D638 |
Lucent Polymers TPP-210 Polypropylene, 10% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |