Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers PPC-0222 Polypropylene, Impact Modified

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Lucent Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers PPC-0222 Polypropylene, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
1/8" Section
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.03 MPa
4501 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Flexural Strength 37.93 MPa
5501 psi
ASTM D790
Flexural Modulus 1.034 GPa
150.0 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.89 °C
120.0 °F
ASTM D648
Users viewing this material also viewed the following: