Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 21.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.4 MPa
3100 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W84598L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Omni Plastics OmniTuff™ CPP CCF30 Copolymer Polypropylene Calcium Carbonate Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Omni Plastics OmniTuff™ HPP CCF40 Homopolymer Polypropylene Calcium Carbonate Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Tensile Strength, Yield 21.4 MPa

@Temperature 121 °C
3100 psi

@Temperature 250 °F
ASTM D638
Network Polymers Nylon 0304NL
Description: Natural NylonInformation provided by Network Polymers Inc.
Tensile Strength, Yield 21.4 MPa
3100 psi
at 100%; ASTM D412
2065D Polyurethane-based Biomedical Elastomer
Tensile Strength, Yield 21.4 MPa
3100 psi
Type I, 2 in/min; ASTM D638
M. Holland Company IS350 Polystyrene, High Impact  (discontinued **)
Uses: Audio Tapes, Structural Foam, Household Goods, Housings, ToysProcessing Method: Injection MoldingInformation provided by M. Holland.
Tensile Strength, Yield 21.4 - 117 MPa
3100 - 17000 psi
Average value: 51.5 MPa Grade Count:20
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
Tensile Strength, Yield 21.4 MPa
3100 psi
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: BK15 is an SBC consisting of our developmental BK10 grade with a mold release added for easier processing. BK15 molded parts give excellent detail on f..
Tensile Strength, Yield 21.4 MPa
3100 psi
Type 1 Specimen, Rate: 2"/min; ASTM D638
Global GPP-2500 Polypropylene Impact Copolymer, Nucleated
Information provided by Global Polymers Corporation.
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE
A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided ..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
JPJ Technologies PP PE35-1 Impact copolymer for Injection Molding
PP M700R is impact copolymer of good fluidity, excellent impact resistance at low temperature, good rigid-tough balance and improves stiffness. Products made from this resin are characterized by fas..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Techmer ES Statiblend® 02020 MB Polypropylene, 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by Weight/Unspecified FillerReinforFeatures: ConductiveTPCI# 9117116Information provided by TP Composites, Inc.
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D 638
Styrolution PS 5801 HIPS
Exceptional processabilityHigh toughnessUSP Class VI certifiedUl Classification 94 HBInformation provided by Styrolution
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D412
Teknor Apex APEX® 3300-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. ..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. ..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Total PPC 5724 Polypropylene, Extra High Impact Copolymer
ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. ..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. ..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp
Applications:Tool handlesToys/sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clar..
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Injection Grade Polystyrene Compounded Resin, Injection Molding
AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness.
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D-638
Axiall 1025-115A Flexible PVC
Non-lead stabilized, 85C rated harness compound formulated for SAE J1128 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 21.4 MPa
3100 psi
2" (50mm) per min; ASTM D638
Formosa Plastics Formolene® L64220U Rotational Molding LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L64220U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase ProcessTM. Th..