Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide 30% Carbon Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | |
Pacific Sintered Materials SS-316-SH 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-SH Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 186 MPa @Strain 0.200 %, Temperature 760 °C |
27000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 5105 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 HS L BK 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated TPCI# 8263101Information provided by TP Composit.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 NAT001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightUL File Number: E157318Appearance: Black and Natural ColorTPCI# 9475101Information provi.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 CF20 TS15 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAdditive: PTFE Lubricant(10%) and Silicone Lubricant Features: Lubricated, Good Wear Resistance and L.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49RS PPA (Europe-Africa-Middle East) LNP* Thermocomp* UFW49RS is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49RSC PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UFW49RSC is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features include: Heat Stabilized. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF/M50 FR 50% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF25 HS NAT 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66 LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66 LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK) Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent .. |
|||
Tensile Strength, Yield | 186 MPa @Temperature 22.8 °C |
27000 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Clariant Renol PA213G50 Nylon 6, 50% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 186 MPa @Strain 0.200 % |
27000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 825 UNS N08825 Nickel Superalloy Uses: Downhole tubulars for deep, corrosive wells. Pollution control, scrubber, and radwaste systems. CPI process piping systems.Property values are for samples in the metallurgical condition: 2100°.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | Dry; ASTM D638 |
Asahi Kasei Leona® 54G43 43% Glass Filled Nylon 66 Enhanced strength, stiffness, and impact resistance; with 43% GF. Excellent appearance. Applications:Fans, railroad tie insulators, office furniture Information provided by Asahi Kasei |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES Luriblend® HTN 01400 BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, .. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES Luriblend® PPA CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | |
PSM Industries Pacific Sintered Metals Invar FN-251-S Powdered Metal Coefficient of thermal expansion equal to glassInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES Electrablend® PA6 CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Conductive, Heat Stabilized and Lubric.. |
|||
Tensile Strength, Yield | 186 MPa | 27000 psi | ASTM D638 |
Techmer ES Electrablend® PA6 E CF20 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Conductive Appearance: Natural ColorProcessing Method: ExtrusionInformation p.. |