Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
PolyOne OnForce™ LFT NN-30 LGF/000 Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced Nylon 66, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PK-30CF/15T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Polymer Resources NY66-G33-[color]-H Nylon 66, 33% Glass Reinforced, Heat Stabilized Nylon 66, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon EE008E PEI LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r.. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF33 L N BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: Fast Molding Cycle and LubricatedAppearance: BlackTPCI# 87.. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF40 L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF30 HS L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 LE BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesAppearance: BlackTPCI#7762101Information provided by TP Compos.. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 SF L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Strontium FerriteFeatures: LubricatedInformation provided by TP .. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Techmer ES HiFill® PEEK GF30 HF 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
Ashley Polymers Ashlene® 980LS-43GB Nylon 612, 43% Glass Reinforced A 43% glass reinforced, heat stabilized Nylon 612 resin in black.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 183 MPa | 26500 psi | ASTM D638 |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |