Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G60T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: This grade is particularly suited to static ap.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D412 |
Precision Polymer Engineering V95X Fluoroelastomer Compound Fluoroelastomer Rubber, 88 - 97 °IRHD. Copolymer of vinylindene fluoride and hexafluoropropylene. Gas-blister resistant fluoroelastomer rubber.Applications: Developed for oil field applications wh.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D412 |
Precision Polymer Engineering Z80B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 75-80 °IRHD. Medium acrylonitrile content (ACN = 33.5%). ASTM designation = HNBR. ASTM D2000 line call-out 4MDH716, A26, B36, EO16, EO36, F14, Z1. Z1 .. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers DEXFLEX® 810HSF TPO
(discontinued **) Description: DEXFLEX® 810HSF is a thermoplastic olefinic elastomer (TPO) designed for large molded-in-color automotive exterior applications that require high flow characteristics for excellent pro.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D638 |
SABIC R50035 Linear Low Density Polyethylene for Rotational Molding Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warp.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | 50 mm/min |
Polimeri Europa EDISTIR PD RR745E High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,088-03-07-12 Environmental stress cracking resistant (ESCR) HIPS. It combines high impact strength with high chemical r.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | 50 mm/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 190-1327 LMDPE Rotational Molding Resin Description: ICORENE 190-1327 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-3522 TO BU 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-3522 TO BU is a 20% talc-filled, elastomer modified, UV-stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3522 TO BU is developed for producing injection m.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | 50mm/min; ASTM D638M-89 |
Micropol Microcene MC121 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ISO 527 |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific) LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D638 |
Tipco Tipcolene® TPE-HMI TPE HMI - Impact Modified Polypropylene Copolymer Compound with High Flow, Soft Touch High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | |
Trelleborg R431 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | |
Trelleborg R483 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | |
Trelleborg R491 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | |
Trelleborg R583 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | At 50 mm/min; ISO 527-2 |
Borealis Daplen™ VB4411 TPO Compound Daplen VB4411 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen VB4411 is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | 50 mm/min cross speed; ASTM D638 |
DuPont™ Surlyn® PC350 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC350 luxury molding resin is a "select" grade of Surlyn® 8945, controlled to achieve the highest possible optical clarity in molded perfume jars and caps, while being optimized for proces.. |
|||
Tensile Strength, Yield | 16.0 MPa @Strain 300 % |
2320 psi @Strain 300 % |
ASTM D412 |
Dow Buna® SB 1502 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1502 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. A non-discoloring stabilizer is added during the production process. Buna® SB 1502 - Sc.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437M20L Mica Reinforced |
|||
Tensile Strength, Yield | 16.0 MPa @Strain 50.0 % |
2320 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W20L Wollastonite Reinforced |
|||
Tensile Strength, Yield | >= 16.0 MPa | >= 2320 psi | ASTM D638 |
Buckeye Polymers BP FLEX D6020 BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | >= 16.0 MPa | >= 2320 psi | ASTM D638 |
Buckeye Polymers BP FLEX D6020 U BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | |
BASF Procom® X10S 773 Polypropylene Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 16.0 MPa | 2320 psi | At 50 mm/min; ISO 527-2 |
Borealis Daplen™ KB4436 TPO Compound Daplen KB4436 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen KB4436 is a material with excellent impact/stiffness ratio. Thanks to its low the.. |