Polymer Property : Tensile Strength, Yield = 13.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.6 MPa
1970 psi
-20% change after 70 hours @ 125°C; ASTM D412
Precision Polymer Engineering E85Q Ethylene Propylene Rubber
Peroxide cured, Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Fo..
Tensile Strength, Yield 13.6 MPa
1970 psi
ASTM D412
Precision Polymer Engineering Z65L Hydrogenated NBR Compound
Peroxide Cured, Hydrogenated Nitrile Rubber, 60-65 °IRHD. Low acrylonitrile content (ACN = 17%). ASTM designation = HNBR.Applications: High strength and excellent chemical resistance. Higher opera..
Tensile Strength, Yield 13.6 MPa
1970 psi
-15% change after 70 hours @ 150°C; ASTM D412
Precision Polymer Engineering Z70F Hydrogenated NBR Compound
Hydrogenated Nitrile Butadiene Rubber (HNBR), 65-75 °IRHD. Medium acrylonitrile content (ACN = 34%). Formulated using only those ingredients determined by the United States Food and Drug Administr..
Tensile Strength, Yield 13.6 MPa
1970 psi
ASTM D412
Polymax® Maxelast® C4990 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Strength, Yield 13.6 MPa
1970 psi
ASTM D638
LyondellBasell Petrothene® NA247000 Low Density Polyethylene, Injection Molding Grade
ApplicationsPetrothene NA247000 provides a balance of stiffness and tear strength. Typical applications include tamper evident caps and closures.Regulatory StatusNA247000 meets the requirements of t..
Tensile Strength, Yield 13.6 MPa
1970 psi
ASTM D638
Entec Hypel® PELD2/.920 LDPE
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..