Precision Polymer Engineering E85Q Ethylene Propylene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering E85Q Ethylene Propylene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Peroxide cured, Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600. ASTM & ISO designation = EPDM.Applications: Excellent water and steam resistance. For repeated use in equipment associated primarily with the production of aqueous foodstuff intended for human consumption.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
90
90
°IRHD, +10 change after 70 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 13.6 MPa
1970 psi
-20% change after 70 hours @ 125°C; ASTM D412
17.0 MPa
2470 psi
ASTM D412
Elongation at Break 111 %
111 %
-40% change after 70 hours @ 125°C; ASTM D412
185 %
185 %
ASTM D412
Compression Set 12 %
12 %
22 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F