Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.40 MPa | 203 psi | ASTM D638 |
Premix Thermoplastics PRESEAL® TPE 5020 General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o.. |
|||
Tensile Strength, Yield | 1.40 MPa | 203 psi | ISO 37 |
Premix Thermoplastics PRESEAL® TPE 5020 General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o.. |
|||
Tensile Strength, Yield | 1.40 MPa | 203 psi | At 100% elongation, across flow; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength, Yield | >= 1.40 MPa | >= 203 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5243 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.40 MPa | 203 psi | at 100% elongation, maximum |
Dow Corning SILASTIC® 37085-V SILICONE RUBBER BLACK 50 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning |
|||
Tensile Strength, Yield | 1.40 MPa | 203 psi | |
ACC MM903 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tensile Strength, Yield | 1.40 MPa | 203 psi | cured 20 mins @150°C |
ACC QLE 1035 QSI Quantum Silicones 38 Durometer Addition Cure Elastomer for Coating QLE 1035 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |