Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.31 MPa | 190 psi | at 200%, as molded |
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.31 MPa | 190 psi | ASTM D412 |
Polymax® Maxelast® P3965H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 1.31 MPa | 190 psi | @50% Elongation; ASTM D1414 |
Greene Tweed FLUORAZ® 888 Fluoroelastomer, FEPM Fluoraz® 888 polytetrafluoroethylene/propylene (FEPM) performs well in aggressive chemicals where ultra pure materials are not required. Recommended for conventional wet and dry system applicatio.. |
|||
Tensile Strength, Yield | 1.31 MPa | 190 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.31 MPa | 190 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.31 MPa | 190 psi | at 100%; ASTM D638 |
Multibase Multi-Flex® A 6221 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsAutomotive Under the HoodInfo.. |
|||
Tensile Strength, Yield | >= 1.31 MPa | >= 190 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7075 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | >= 1.31 MPa | >= 190 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7267 Ethylene-Propylene Rubber EPDM for high temperature steam service. Also available as a Y267-Type (7267L).Information provided by Seals Eastern, Inc. |