Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor LT74104 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74104 is a high strength linear low density polyethylene containing no slip or antiblock. It is designed for blown film applications and is well suited for consumer an.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor LT74105 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74105 is a high strength linear low density polyethylene containing medium slip and medium antiblock. It is designed for blown film applications and is well suited for.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor LT74113 Hexene Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74113 is a high strength hexene linear low density polyethylene containing no slip and medium antiblock. It is designed for blown film applications and is well suited .. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor LT74119 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74119 is a high strength linear low density polyethylene containing medium slip and high antiblock and it contains processing aid. It is designed for blown film applic.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor LT74147 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74147 is a high strength linear low density polyethylene containing medium slip and high antiblock. It is designed for blown film applications and is well suited for c.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74838 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and medium antiblock. Films produced with this re.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor Xtreme SC74842 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74842 polymer is a high strength and good clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. Films produced wit.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor Xtreme SC74845 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74845 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and high antiblock. Films produced with this resi.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Hifor Xtreme SC74849 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme Polyethylene SC74849 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock, and polymer processing aid.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake LF2050 Hexene Linear Low Density Polyethylene Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
ExxonMobil LLDPE LL 1004YB Film Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1004YB is an LLDPE grade, offering excellent high temperature stability. Properties may be further enhanced by the combination with Exceed mLLDPE. Availability: Africa & Midd.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
ExxonMobil LLDPE LL 3404.48 Linear Low Density Polyethylene Resin Product Description: LL 3404.48 is a hexane medium density polyethylene cast film grade for applications requiring high strength and high stiffness. Films produced from this resin exhibit good tensi.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
Dow DX5E66 Polypropylene Homopolymer Resin OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P.. |
|||
Film Tensile Strength at Break, MD | 50.3 MPa | 7300 psi | ASTM D882 |
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. .. |