Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene
ApplicationsPETROTHENE NA 285-003 is a medium density polyethylene resin for blown or cast film extrusion. Typical applications include overwrap film. This product exhibits good film optics and hi..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
Westlake EF403 Low Density Polyethylene
WESTLAKE polyethylene EF403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent skrinkability, and has very good optic..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
Westlake EF603 Low Density Polyethylene
Westlake EF603 is a LDPE resin with excellent toughness and processability. It is suggested in heavy duty films and medium duty shrink applications. It can be used as a bubble stabilizer in LLDPE ri..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil Escorene™ FL 00212 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00212 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 260°C (500°F) may cause resin degradation. Machines should always b..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00112 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applica..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil LDPE LD 156BW Low Density Polyethylene Resin
Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil LDPE LD 156HE Low Density Polyethylene Resin
Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin
Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin
Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin
Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin
Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A..
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
ExxonMobil Escorene™ FL 00112 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00112 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No App..
Copyright © lookpolymers.com All Rights Reserved