Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | >= 172 MPa | >= 25000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 473 Polyester Film, 200 Gauge Melinex® 473 is a high clarity polyester film manufactured with a coating on one surface that improves slip and handling characteristics. The opposite surface is raw polyester (non-coated). The sli.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 513P Polyester Film, 650 Gauge Melinex® 513P is a high clarity, knurled film with excellent handling properties that is pretreated on both sides to promote adhesion to most industrial coatings.General Product Info: Melinex® 513.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 515 Polyester Film A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brilliance.Typical Applications: MELINEX® 515 is suitable for applications which .. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 623 Polyester Film, 750 Gauge Melinex® 623 is a super clear polyester film pretreated on both surfaces to give superior solvent adhesion and improved handleability.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 680 Polyester Film, 750 Gauge Melinex® 680 is a super clear polyester film, pretreated on one side to promote adhesion with improved handleability. It is high clarity, non-yellow base with excellent adhesion on the pretreated s.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Melinex® WCW Polyester Film, 200 Gauge Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Melinex® WCW Polyester Film, 75 Gauge Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Melinex® WCW Polyester Film, 92 Gauge Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® E Polyester Film, 142 Gauge Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® E Polyester Film, 92 Gauge Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® M461 Polyester Film, 142 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® M461 Polyester Film, 200 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® M461 Polyester Film, 48 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® M461 Polyester Film, 500 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® M461 Polyester Film, 92 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OB13AF Polyester Film, 100 Gauge Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OB13AF Polyester Film, 150 Gauge Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OL2 Polyester Film, 75 Gauge Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge Product Description: Mylar® OWF2 is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. Mylar® OWF2 has a thicker heat sealable layer than Myla.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge Product Description: Mylar® RB42AF is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer and polyvinylidene chloride (PVdC) layer on the opposite side. .. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RB43 Polyester Film, 100 Gauge Mylar® RB43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite side. Mylar® R.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge Product Description: Mylar® RB52 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opp.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RL31 Polyester Film, 100 Gauge Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RL31 Polyester Film, 75 Gauge Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RSX Polyester Film, 105 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RSX Polyester Film, 300 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RSX Polyester Film, 48 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RSX Polyester Film, 500 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® M461 Polyester Film, 300 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RSX Polyester Film, 200 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |