Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 145 MPa | 21000 psi | ExxonMobil Method |
ExxonMobil Bicor® 100 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Film Tensile Strength at Break, MD | 145 MPa | 21000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 25ICT OPP Film Product Description: A one-side sealable, very broad seal range coextruded BOPP. This film is designed for use in unsupported plain or surface printed high-speed horizontal applications. The enhance.. |
|||
Film Tensile Strength at Break, MD | 145 MPa | 21000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Metallyte™ 30MM680 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS .. |
|||
Film Tensile Strength at Break, MD | 145 MPa | 21000 psi | ASTM D882A |
DuPont Teijin Films Mylar® WRL63 Polyester Film, 200 Gauge Mylar® WRL63 is a biaxially oriented polyester (OPET) film with a modified ethylene acrylate heat seal layer. It provides peelable seal over a broad temperature range to a number of bottles or cont.. |