Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 234 - 283 MPa | 34000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Film Tensile Strength at Break, MD | 234 - 283 MPa | 34000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ MT2500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited fo.. |