Film Tensile Strength at Break, MD >= 58.6 MPa
>= 8500 psi
ASTM D 882 A
Total Finathene® 2344 HDPE film  (discontinued **)
Applications: Trash can liners, merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
LyondellBasell Alathon® L5005 High Density Polyethylene
ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Westlake Hifor Xtreme SC74844 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74844 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip, high antiblock and processing aid. Films produce..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Westlake Hifor Xtreme SC74853 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74853 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and processing aid. Films produced wi..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Westlake Hifor Xtreme SC74858 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74858 polymer is a high strength, good clarity linear low density polyethylene designed for blown film extrusion that contains no slip or antiblock and processing aid. Films ..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin
Product Description: Enable 27-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
ExxonMobil LL 3003.32 Cast Film Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
ExxonMobil LL 3003.39 Cast Film Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP)
AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Dow DOWLEX™ 2025G Linear Low Density Polyethylene
DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp..
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Copyright © lookpolymers.com All Rights Reserved