Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene ApplicationsPETROTHENE NA 285-003 is a medium density polyethylene resin for blown or cast film extrusion. Typical applications include overwrap film. This product exhibits good film optics and hi.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
Westlake EF403 Low Density Polyethylene WESTLAKE polyethylene EF403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent skrinkability, and has very good optic.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
Westlake EF603 Low Density Polyethylene Westlake EF603 is a LDPE resin with excellent toughness and processability. It is suggested in heavy duty films and medium duty shrink applications. It can be used as a bubble stabilizer in LLDPE ri.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00212 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00212 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 260°C (500°F) may cause resin degradation. Machines should always b.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00112 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applica.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil LDPE LD 156BW Low Density Polyethylene Resin Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil LDPE LD 156HE Low Density Polyethylene Resin Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A.. |
|||
Film Tensile Strength at Break, MD | 30.3 MPa | 4400 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00112 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00112 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No App.. |