Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 375 g | 375 g | ASTM D1922 |
NOVA Chemicals Surpass® FPs317-A Octene sLLDPE Film Resin Features: Exceptional puncture resistanceVery good tear propertiesLow gel levelExcellent optical properties Excellent elongation characteristics Easy to process, no drying required Applications: Cas.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | ASTM D1922 |
Formosa Plastics Formolene® FORMAX® L71709A Film (Hexene Grade) LLDPE
(discontinued **) High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | ASTM D1922 |
Formosa Plastics Formolene® FORMAX® L71709E2 Film (Hexene Grade) LLDPE
(discontinued **) High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | ASTM D1922 |
Formosa Plastics Formolene® FORMAX® L71709H Film (Hexene Grade) LLDPE
(discontinued **) High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | ASTM D1922 |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | |
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 .. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | ASTM D-1922 |
Bapolene® 142A Polyethylene Film Grade Bapolene 142A is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | ASTM D-1922 |
Bapolene® 142B Polyethylene Film Grade Bapolene 142B is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Elmendorf Tear Strength MD | 375 g | 375 g | ASTM D-1922 |
Bapolene® 142F Polyethylene Film Grade Bapolene 142F is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |