Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 11.4 MPa | 1650 psi | ASTM D882 |
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength, 0.7 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Film Tensile Strength at Yield, MD | 11.4 MPa | 1650 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 071.MU Blown Film Resin
(discontinued **) LD 071 series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, toughness, burn-through re.. |
|||
Film Tensile Strength at Yield, MD | 11.4 MPa | 1650 psi | |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |
|||
Film Tensile Strength at Yield, MD | 11.4 MPa | 1650 psi | ASTM D882 |
Dow DOWLEX™ 2085G Polyethylene Resin DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in ot.. |
|||
Film Tensile Strength at Yield, MD | 11.4 MPa | 1650 psi | |
Dow Elite® 5100 Linear Low Density Polyethylene 5100 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and puncture pro.. |
|||
Film Tensile Strength at Yield, MD | 11.4 MPa | 1650 psi | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Film Tensile Strength at Yield, MD | 11.4 MPa | 1650 psi | |
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an.. |
|||
Film Tensile Strength at Yield, MD | 11.4 MPa | 1650 psi | |
Dow LDPE 493A Low Density Polyethylene, Film Grade DOW LDPE 493A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 493A resin can be blended with most linear low density.. |