Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength, 0.7 mil Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength, 0.7 mil Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior properties along with the resin's good drawdown capability permit usage in many demanding packaging applicationsApplications: Merchandise bags; Frozen food packaging; Heavy duty bags; Sandwich bags; Liners. Data for film properties below based on 0.7 mil film.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
Exxon Method
Thickness 17.8 microns
0.700 mil
Melt Flow 1.3 g/10 min
1.3 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.4 MPa
1650 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.9 MPa
1730 psi
ASTM D882
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 690 %
690 %
ASTM D882
Secant Modulus, MD 0.226 GPa
32.8 ksi
ASTM D882
Secant Modulus, TD 0.276 GPa
40.0 ksi
ASTM D882
Elmendorf Tear Strength MD 190 g
190 g
ASTM D1922
Elmendorf Tear Strength TD 720 g
720 g
ASTM D1922
Elmendorf Tear Strength, MD 10.7 g/micron
271 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 40.51 g/micron
1029 g/mil
ASTM D1922
Dart Drop 5.63 g/micron
143 g/mil
F50; ASTM D1709
Dart Drop Test 100 g
0.221 lb
F50; ASTM D-1709
Film Tensile Strength at Break, MD 57.6 MPa
8350 psi
ASTM D882
Film Tensile Strength at Break, TD 38.6 MPa
5600 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
Exxon Method
Optical Properties Metric English Comments
Haze 30.4 %
30.4 %
ASTM D1003
Gloss 24 %
24 %
45°, ASTM D-2457
Users viewing this material also viewed the following: