Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 1311 Polyester Film Melinex® 1311 is a clear polyester film with antistatic properties on both surfaces for improved web handling and safety.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 378 Polyester Film Melinex® 378 is a translucent, matte, polyester film which has a rougher surface (lower surface gloss) than Melinex® 377.Approvals: UL Recognition - Product has been registered with Underwriters L.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 437 Polyester Film, 200 Gauge Melinex® 437 is a two side differentially pretreated super clear film; 1 side promotes adhesion, 1 side slip.Also available in 270, 370, 465, 650 GaugeInformation provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 142 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 200 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 400 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 92 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 400 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 500 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 92 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 456 Polyester Film Melinex® 456 is an excellent handling, high clarity polyester film with both sides pretreated for slip. The two smooth surfaces allow easy top coating.Approvals: UL 94 VTM-2 - for 200 - 700 gauge (.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 505 Polyester Film Melinex® 505 is a high clarity polyester film which is pretreated on both sides to promote adhesion to most industrial coating and inks.Approvals: UL 94 VTM-2 - for 1000 gauge (0.26mm) onlyInformat.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 561 Polyester Film Melinex® 561 is a high clarity polyester film which is pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 561 is suitable for applications which require a .. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 595 Polyester Film, 400 Gauge Melinex® 595 is a high clarity film that is one side pretreated to provide anti-charge protection and one side pretreated to promote adhesion to many solvent coating formulations. This film is exce.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 965 Polyester Film, 500 Gauge Melinex® 965 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 966 Polyester Film, 700 Gauge Melinex® 966 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® FRPS Polyester Film, 142 Gauge Melinex® FRPS is a lower shrinkage version of Melinex® S. Designed specifically for release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and .. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® WCW Polyester Film, 200 Gauge Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® WCW Polyester Film, 92 Gauge Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 142 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 275 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 400 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 500 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 700 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 516 Polyester Film Melinex® 516 is a high clarity polyester film which is pretreated on both sides for slip to combine good handling properties with high clarity and brilliance.Typical Applications: Some typical uses.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 535 Polyester Film Melinex® 535 is a high clarity polyester film that is two-side pretreated to promote adhesion to aqueous based coatings.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 943 Polyester Film Melinex® 943 is a super clear film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 200 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 300 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, MD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 457 Polyester Film, 200 Gauge Melinex® 457 is one side slip, one side adhesion promoting, super clear, polyester film for color proof applications.Also available in 650 gaugeInformation provided by DuPont. |