Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data) Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein.. |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f.. |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor applied; QTM 55010 |
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.140 - 1.10 MPa-m/sec | 4000 - 31400 psi-ft/min | Average value: 0.556 MPa-m/sec Grade Count:6 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |