Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 506 MPa @Strain 0.200 %, Temperature 871 °C |
73400 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes R-41 alloy, 0.635 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Tensile Strength, Yield | 506 MPa @Temperature 23.0 °C |
73400 psi @Temperature 73.4 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |