Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 379 MPa @Temperature 138 °C |
55000 psi @Temperature 280 °F |
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Tensile Strength, Yield | 379 MPa @Thickness 1.57 mm |
55000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP555 Carbon Fiber
(discontinued **) Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane m.. |
|||
Tensile Strength, Yield | >= 379 MPa @Diameter 3.17 - 10.319 mm, Strain 0.200 % |
>= 55000 psi @Diameter 0.125 - 0.40625 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Pure Molybdenum AB, Arc-Cast Bar Arc-Cast BarDescription of Product: This specification covers carbon-deoxidized molybdenum wrought bar produced from ingots consolidated by the H.C. Stark consumable electrode vacuum-arc-casting pr.. |
|||
Tensile Strength, Yield | >= 379 MPa @Diameter 73.03 - 88.9 mm, Strain 0.200 % |
>= 55000 psi @Diameter 2.875 - 3.50 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Pure Molybdenum AB, Arc-Cast Bar Arc-Cast BarDescription of Product: This specification covers carbon-deoxidized molybdenum wrought bar produced from ingots consolidated by the H.C. Stark consumable electrode vacuum-arc-casting pr.. |
|||
Tensile Strength, Yield | >= 379 MPa @Diameter 3.17 - 10.319 mm, Strain 0.200 % |
>= 55000 psi @Diameter 0.125 - 0.40625 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Pure Molybdenum ABL, Arc-Cast, Low Carbon Bar Description of Product: This specification covers carbon-deoxidized, low-carbon molybdenum wrought bar produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting p.. |
|||
Tensile Strength, Yield | >= 379 MPa @Diameter 73.03 - 88.9 mm, Strain 0.200 % |
>= 55000 psi @Diameter 2.875 - 3.50 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Pure Molybdenum ABL, Arc-Cast, Low Carbon Bar Description of Product: This specification covers carbon-deoxidized, low-carbon molybdenum wrought bar produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting p.. |
|||
Tensile Strength, Yield | 379 MPa @Thickness 6.35 mm, Temperature 20.0 °C |
55000 psi @Thickness 0.250 in, Temperature 68.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | 379 MPa @Strain 2.00 %, Temperature 21.1 °C |
55000 psi @Strain 2.00 %, Temperature 70.0 °F |
|
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability .. |
|||
Tensile Strength, Yield | 379 MPa @Strain 0.200 % |
55000 psi @Strain 0.200 % |
Bar |
Special Metals INCONEL® alloy 22 Austenitic Alloy INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat.. |
|||
Tensile Strength, Yield | 379 - 552 MPa @Strain 0.200 % |
55000 - 80000 psi @Strain 0.200 % |
Annealed Bar |
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan.. |
|||
Tensile Strength, Yield | 379 MPa @Temperature 24.0 °C |
55000 psi @Temperature 75.2 °F |
Warp TS |
Hexcel® HexPly® F185 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F185; Fiber: 150-1/2Information provided by HexCel |
|||
Tensile Strength, Yield | 379 MPa @Temperature 71.0 °C |
55000 psi @Temperature 160 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F522; Fiber: 75-1/0Information provided by HexCel |
|||
Tensile Strength, Yield | 379 MPa @Strain 0.200 % |
55000 psi @Strain 0.200 % |
Annealed |
AK Steel 201 Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Tensile Strength, Yield | 379 MPa @Strain 0.200 % |
55000 psi @Strain 0.200 % |
Annealed |
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Tensile Strength, Yield | 379 MPa @Temperature 249 °C |
55000 psi @Temperature 480 °F |
Annealed |
ATI Wah Chang TI-3Al-2.5V Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working an.. |
|||
Tensile Strength, Yield | 379 MPa @Diameter 25.4 mm, Temperature 25.0 °C |
55000 psi @Diameter 1.00 in, Temperature 77.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | 379 MPa @Diameter 50.8 mm, Temperature 25.0 °C |
55000 psi @Diameter 2.00 in, Temperature 77.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |