Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 35.0 MPa @Temperature 77.0 °C |
5080 psi @Temperature 171 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 35.0 MPa @Temperature 200 °C |
5080 psi @Temperature 392 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Tensile Strength, Yield | 35.0 MPa @Temperature 23.0 °C |
5080 psi @Temperature 73.4 °F |
90° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 35.0 MPa @Temperature 80.0 °C |
5080 psi @Temperature 176 °F |
ASTM D638 |
BASF Ultramid® 8202 L Intermediate PA6 (Dry) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |