Mechanical Properties Metric English Comments
Tensile Strength, Yield 330 MPa

@Strain 1.00 %
47900 psi

@Strain 1.00 %
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 330 MPa

@Strain 1.00 %
47900 psi

@Strain 1.00 %
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel
Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro..
Tensile Strength, Yield 330 MPa

@Strain 0.200 %,
Temperature 100 °C
47900 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Yield >= 330 MPa

@Strain 1.00 %
>= 47900 psi

@Strain 1.00 %
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42
Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0...
Tensile Strength, Yield 330 MPa

@Temperature 177 °C
47900 psi

@Temperature 351 °F
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel
Tensile Strength, Yield 330 MPa

@Temperature 93.0 °C
47900 psi

@Temperature 199 °F
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric
Information provided by HexCel
Tensile Strength, Yield 330 MPa

@Strain 0.200 %,
Thickness 152.4 - 203.2 mm
47900 psi

@Strain 0.200 %,
Thickness 6.000 - 8.000 in
Typical Strength
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
Tensile Strength, Yield >= 330 MPa

@Strain 0.200 %,
Thickness 203.2 - 254 mm
>= 47900 psi

@Strain 0.200 %,
Thickness 8.000 - 10.0 in
Tempers T651 / T652
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Tensile Strength, Yield >= 330 MPa

@Strain 0.200 %,
Thickness 60.0 - 80.0 mm
>= 47900 psi

@Strain 0.200 %,
Thickness 2.36 - 3.15 in
Temper T651
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..
Tensile Strength, Yield >= 330 MPa

@Strain 0.200 %,
Thickness 80.0 - 120 mm
>= 47900 psi

@Strain 0.200 %,
Thickness 3.15 - 4.72 in
Temper T651
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..
Tensile Strength, Yield 330 MPa

@Strain 1.00 %
47900 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..
Tensile Strength, Yield 330 MPa

@Strain 0.200 %,
Temperature 200 °C
47900 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..