Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.0 MPa @Temperature 121 °C |
4790 psi @Temperature 250 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 33.0 MPa @Strain 300 % |
4790 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1055D Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 33.0 MPa @Strain 300 % |
4790 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 3065D Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 33.0 MPa @Strain 300 % |
4790 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1065D Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 33.0 MPa @Strain 300 % |
4790 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1160D Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 33.0 MPa @Temperature 23.0 °C |
4790 psi @Temperature 73.4 °F |
ASTM D638 |
BASF Ultramid® 8281 HS GP PA6 (Conditioned) Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p.. |
|||
Tensile Strength, Yield | 33.0 MPa @Strain 300 % |
4790 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® 1160D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh.. |
|||
Tensile Strength, Yield | 33.0 MPa @Strain 300 % |
4790 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhi.. |