Material Notes:
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These products can be injection molded, blow molded, and extruded.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength 40.0 MPa
5800 psi
ASTM D412
Tensile Strength, Yield 16.0 MPa

@Strain 50.0 %
2320 psi

@Strain 50.0 %
ASTM D412
19.0 MPa

@Strain 100 %
2760 psi

@Strain 100 %
ASTM D412
33.0 MPa

@Strain 300 %
4790 psi

@Strain 300 %
ASTM D412
Elongation at Break 370 %
370 %
ASTM D412
Tear Strength 1050 kN/m
5990 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 70
70
ASTM D1044(Taber) H-22
Compression Set 30 %

@Temperature 23.0 °C,
Time 79200 sec
30 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395