Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 305 MPa @Temperature 20.0 °C |
>= 44200 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Tensile Strength, Yield | 305 MPa @Strain 1.00 % |
44200 psi @Strain 1.00 % |
Typical |
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |
|||
Tensile Strength, Yield | 305 MPa @Strain 1.00 % |
44200 psi @Strain 1.00 % |
Typical after Solution Annealing |
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se.. |
|||
Tensile Strength, Yield | 305 MPa @Strain 0.200 %, Thickness 8.00 - 25.0 mm |
44200 psi @Strain 0.200 %, Thickness 0.315 - 0.984 in |
Typical Strength; Standard EN 485-2 |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength, Yield | 305 MPa @Strain 0.200 %, Thickness 4.99 - 20.0 mm |
44200 psi @Strain 0.200 %, Thickness 0.196 - 0.787 in |
Typical Strength |
Constellium Planoxal® 60 Aluminum plate The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use.. |
|||
Tensile Strength, Yield | 305 MPa @Strain 0.200 %, Thickness 9.90 - 25.0 mm |
44200 psi @Strain 0.200 %, Thickness 0.390 - 0.984 in |
Typical Strength |
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |
|||
Tensile Strength, Yield | 305 MPa @Strain 0.200 % |
44200 psi @Strain 0.200 % |
Typical |
Aleris Weldural Aluminum Alloy, 400 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Tensile Strength, Yield | 305 MPa @Thickness 3.00 mm |
44200 psi @Thickness 0.118 in |
L Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |
|||
Tensile Strength, Yield | 305 MPa @Thickness 7.00 mm |
44200 psi @Thickness 0.276 in |
L Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |
|||
Tensile Strength, Yield | 305 MPa @Thickness 3.00 mm |
44200 psi @Thickness 0.118 in |
LT Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |
|||
Tensile Strength, Yield | 305 MPa @Thickness 7.00 mm |
44200 psi @Thickness 0.276 in |
LT Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |
|||
Tensile Strength, Yield | >= 305 MPa @Strain 0.200 % |
>= 44200 psi @Strain 0.200 % |
Minimum |
Aleris Weldural Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Tensile Strength, Yield | 305 MPa @Strain 1.00 % |
44200 psi @Strain 1.00 % |
Typical |
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k.. |