Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 30.0 MPa @Temperature 23.0 °C |
4350 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Tensile Strength, Yield | 30.0 MPa @Temperature 77.0 °C |
4350 psi @Temperature 171 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 30.0 MPa @Temperature -30.0 °C |
4350 psi @Temperature -22.0 °F |
ASTM D638 |
Borealis Borstar® HE6081 Black Track Resistant HD Polyethylene Based Compound for Jacketing of Fiber Optical Cable Borstar HE6081 is based on high-density polyethylene and has a specially designed additive package to give excellent track resistance. It is also well protected against UV degradation in order to e.. |
|||
Tensile Strength, Yield | 30.0 MPa @Temperature 80.0 °C |
4350 psi @Temperature 176 °F |
ASTM D638 |
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |
|||
Tensile Strength, Yield | 30.0 MPa @Strain 300 % |
4350 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® 1154D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh.. |
|||
Tensile Strength, Yield | 30.0 MPa @Strain 300 % |
4350 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® M95A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |