Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 220 MPa @Strain 0.200 %, Temperature 100 °C |
31900 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 % |
31900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4303 Cr-Ni Austenitic Stainless Steel Good corrosion resistance with excellent drawing properties.Applications: Suitable for cold formed components where good workability is required. Fasteners, studs.Available in hot rolled plate (Qua.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 %, Temperature -80.0 °C |
31900 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 % |
31900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 % |
31900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 % |
31900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 % |
31900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 % |
31900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 % |
31900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | >= 220 MPa @Temperature 200 °C |
>= 31900 psi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | >= 220 MPa @Strain 0.200 % |
>= 31900 psi @Strain 0.200 % |
|
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
Tensile Strength, Yield | >= 220 MPa @Strain 0.200 % |
>= 31900 psi @Strain 0.200 % |
|
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co.. |
|||
Tensile Strength, Yield | >= 220 MPa @Strain 0.200 % |
>= 31900 psi @Strain 0.200 % |
|
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for sp.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 %, Temperature 982 °C |
31900 psi @Strain 0.200 %, Temperature 1800 °F |
Transverse |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength, Yield | 220 - 280 MPa @Strain 0.200 % |
31900 - 40600 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 220 BH High-strength Steel High-strength SteelComments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is ap.. |
|||
Tensile Strength, Yield | >= 220 MPa @Strain 0.200 %, Thickness 8.00 - 25.0 mm |
>= 31900 psi @Strain 0.200 %, Thickness 0.315 - 0.984 in |
Temper T651 |
Constellium DOKIMA® Rolled Plate Aluminum DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct.. |
|||
Tensile Strength, Yield | >= 220 MPa @Strain 0.200 %, Thickness 25.0 - 60.0 mm |
>= 31900 psi @Strain 0.200 %, Thickness 0.984 - 2.36 in |
Temper T651 |
Constellium DOKIMA® Rolled Plate Aluminum DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct.. |
|||
Tensile Strength, Yield | >= 220 MPa @Strain 0.200 %, Thickness 60.0 - 150 mm |
>= 31900 psi @Strain 0.200 %, Thickness 2.36 - 5.91 in |
Temper T651 |
Constellium DOKIMA® Rolled Plate Aluminum DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct.. |