Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1520 MPa @Strain 0.200 % |
220000 psi @Strain 0.200 % |
52 HRC |
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re.. |
|||
Tensile Strength, Yield | 1517 MPa @Temperature -54.0 °C |
220000 psi @Temperature -65.2 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel |
|||
Tensile Strength, Yield | 1520 MPa @Temperature 20.0 °C |
220000 psi @Temperature 68.0 °F |
52 HRC |
EDRO #5 H13-Hot Work Tool Steel EDRO #5™ H13 is a chromium-molybdenum-vanadium-alloyed steel characterized by: good resistance to thermal shock and thermal fatigue, good high-temperature strength, good toughness and ductility, go.. |
|||
Tensile Strength, Yield | 1520 MPa @Strain 0.200 % |
220000 psi @Strain 0.200 % |
hardened to 52 HRC |
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard.. |
|||
Tensile Strength, Yield | 1520 MPa @Strain 0.200 % |
220000 psi @Strain 0.200 % |
hardness of 52 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Tensile Strength, Yield | 1520 MPa @Strain 0.200 % |
220000 psi @Strain 0.200 % |
hardness of 52 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Tensile Strength, Yield | 1517 MPa @Temperature 23.0 °C |
220000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |