Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 125 MPa @Strain 1.00 %, Temperature 400 °C |
18100 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 125 MPa @Strain 0.200 %, Temperature 400 °C |
18100 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 125 MPa @Temperature 150 °C |
18100 psi @Temperature 302 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in .. |
|||
Tensile Strength, Yield | 125 MPa @Temperature 40.0 °C |
18100 psi @Temperature 104 °F |
ISO 527 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Strength, Yield | 125 MPa @Temperature -40.0 °C |
18100 psi @Temperature -40.0 °F |
ASTM D638 |
BASF Ultramid® 8202 L Intermediate PA6 (Dry) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |