Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
DIN 53.504
Lubrizol Advanced Materials Pearlcoat® 125KW Thermoplastic Polyurethane Elastomer  (discontinued **)
Pearlcoat® D125KW is a polyester-based aromatic TPU, supplied in form of white-colored pellets, combining hardness with excellent low-temperature flexibility.Applications: Pearlcoat® D125KW is us..
Tensile Strength, Yield 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1198A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 2095A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength, Yield 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 3080A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 3080AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tensile Strength, Yield 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 3095A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1080A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1095A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
0.76 mm (0.030 in) extruded sheet; ASTM D-412
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tensile Strength, Yield 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® S90A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue..
Tensile Strength, Yield 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® 685A10 Polyester Type Polyurethane Elastomer
This grade contains a hydrolytic stabilizer. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are ..
Copyright © lookpolymers.com All Rights Reserved