Material Notes:
Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ASTM D2240
Hardness, Shore D 41
41
ASTM D2240
Tensile Strength, Ultimate 37.0 MPa
5370 psi
ASTM D412
Tensile Strength, Yield 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
ASTM D-412
20.0 MPa

@Strain 300 %
2900 psi

@Strain 300 %
ASTM D-412
Elongation at Break 540 %
540 %
ASTM D412
Tear Strength 125 kN/m
713 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 25
25
H-18 wheel; ASTM D-1044.
Tensile Set 55 %
55 %
at break; ASTM D-412